Beilstein J. Nanotechnol. 2017, 8, 203–209, doi:10.3762/bjnano.8.22
Figure 1: A 60 µm thick polydimethylsiloxane (PDMS) membrane with a 400 nm period and 140 nm deep linear grat...
Figure 2: Resonance spectra with crossed polarization filters at a) 0% strain for samples with 2 wt % to 12 w...
Figure 3: The shift of the resonance wavelength for 6 different samples with particle concentrations in the d...
Figure 4: CIE values of the spectra of four different samples (2 to 8% TiO2) for strain values of 0 to 20% pe...
Figure 5: Photographs of the 6 wt % TiO2 sample at strain values of 0 to 20% taken with crossed polarization ...
Figure 6: Fabrication of the flexible photonic crystal membrane by molding and imprinting a PDMS membrane wit...
Figure 7: Cross-section of a 400 nm grating on a PDMS membrane with a particle layer created by a 6 wt % solu...
Figure 8: The measurement setup consists of a transmission light microscope with crossed polarization filters...